Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 35.4 kV/mm | 900 kV/in | Method A; ASTM D149 |
S&E Specialty Polymers TufShield™ FS-1000H-UVFG Insulating Compound Application: A UV and fungus resistant lead-free, low smoke generating, highly flame retardant jacketing and insulation compound designed for Plenum cable application. Compound exhibits excellent pr.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon Thermabond® R37340X008 Primerless Electronic Adhesive
(discontinued **) Liner: 1 mil FEP; Product: uncured Silicone Rubber; Carrier: 3 mil PTFE coated fiberglas |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | Short Time; 1/8 inch; ASTM D149 |
G-11 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D419 |
Teknor Apex Telcar® TL-1522G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D419 |
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
Tra-Con Tra-Bond 293-1 General Purpose Instrument Epoxy Adhesive TRA-BOND 293-1 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293-se.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
Tra-Con Tra-Bond 293-1M General Purpose Instrument Epoxy Adhesive TRA-BOND 293-1M general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper and brass. The 293-se.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | High Humidity; ASTM D1000 |
3M 1400 Economy Vinyl Electrical Tape 3M™ Economy Vinyl Electrical Tape 1400 is a black 7 mil thick, general use vinyl-insulating tape. It is designed to perform continuously in temperatures up to 80°C. This tape has a polyvinyl chlor.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon R34572R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 1080 Style FiberglassAppearance: Red silicone rubber on fiberglass clothThis data represents typical value.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon R37053W007 0.007" (0.178 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1 Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 2133 FiberglassSide 2: Cured Silicone RubberSide 2 Interleave: PolyethyleneThis data represents ty.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon Thermabond® 99A90X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon 48B12R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be used.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
3M 93020LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
3M Scotch® FP-301 Heat Shrink Tubing Scotch® Heat Shrink Tubing FP-301 offers an outstanding balance of electrical, physical and chemical properties for a wide variety of industrial and military applications. Rated for 135°C continuo.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
3M Scotch® FP-301VW Heat Shrink Tubing Scotch® Heat Shrink Tubing FP-301VW has the same outstanding balance of electrical, physical and chemical properties as FP-301 tubing, and is specially engineered for excellent flame resistance. FP.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
3M TMW Tubing 3M TMW Tubing is a semi-rigid translucent heat-shrinkable polyolefin tubing that is co-extruded and selectively cross-linked with an integral, meltable inner wall. When heated in excess of 135°C th.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | |
3M MW Heat Shrink Tubing 3M Heat Shrink Tubing MW is a semi-rigid, 110°C heat-shrinkable polyolefin tubing that is a co-extruded and selectively cross-linked to provide an integral, meltable inner wall. When heated in exce.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
Arlon Thermabond® 99A90N008 Primerless Electronic Adhesive
(discontinued **) Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer. |
|||
Dielectric Strength | 35.4 kV/mm @Thickness 1.60 mm |
900 kV/in @Thickness 0.0630 in |
ASTM D149 |
Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer
(discontinued **) XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder tempe.. |
|||
Dielectric Strength | 35.4 kV/mm | 900 kV/in | ASTM D149 |
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |