Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer  (discontinued **)

Category Polymer , Thermoplastic , Liquid Crystal Polymer (LCP)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder temperatures. The heat deflection temperature of this resin is 568°F (298°C) and the moldability is exceptional. XYDAR G-430 resin can fill very thin walls over long flow lengths with little or no flash, even at mold temperatures below 200°F (93°C). In addition, it has low warpage in molded products and exceptional weld line strength.Like other XYDAR Liquid Crystal Polymers, this material exhibits high strength and stiffness (even at elevated temperatures), low coefficient of thermal expansion, high deflection temperature, inherent flame resistance, and outstanding resistance to most chemicals, weathering, and radiation.This resin is particularly well suited for many applications that have difficult-to-fill geometries, and require resistance to warp, strong weld lines, and compatibility with IR reflow environments. Potential applications for this resin include electronic connectors, surface mount interconnection devices, sockets, and PCMCIA card frames.Information provided by Solvay Advanced Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.63 g/cc
1.63 g/cc
ASTM D792
Water Absorption <= 0.010 %
<= 0.010 %
24 hours; ASTM D570
Linear Mold Shrinkage, Flow 0.00070 cm/cm
0.00070 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0038 cm/cm
0.0038 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 135 MPa
19600 psi
ASTM D638
Elongation at Break 1.3 %
1.3 %
ASTM D638
Tensile Modulus 15.9 GPa
2300 ksi
ASTM D638
Flexural Strength 184 MPa
26700 psi
ASTM D570
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D570
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Izod Impact Unnotched 8.13 J
6.00 ft-lb
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow -0.900 µm/m-°C

@Temperature 20.0 °C
-0.500 µin/in-°F

@Temperature 68.0 °F
ASTM E831
CTE, linear, Transverse to Flow 54.0 µm/m-°C

@Temperature 20.0 °C
30.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 298 °C
568 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Constant 4.2

@Frequency 100 Hz
4.2

@Frequency 100 Hz
ASTM D150
Dielectric Strength 35.4 kV/mm

@Thickness 1.60 mm
900 kV/in

@Thickness 0.0630 in
ASTM D149
Dissipation Factor 0.0106

@Frequency 100 Hz
0.0106

@Frequency 100 Hz
ASTM D150
Processing Properties Metric English Comments
Melt Temperature 321 - 360 °C
610 - 680 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 149 °C
300 °F
Dry Time 6 - 8 hour
6 - 8 hour
Dew Point -28.9 °C
-20.0 °F