Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.7 kV/mm @Thickness 1.00 mm |
373 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive. |
|||
Dielectric Strength | 14.7 kV/mm @Thickness 1.00 mm |
373 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 compound |
|||
Dielectric Strength | 14.7 kV/mm @Thickness 1.00 mm |
373 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 compound |
|||
Dielectric Strength | 14.7 - 18.9 kV/mm | 373 - 480 kV/in | Average value: 16.9 kV/mm Grade Count:9 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Dielectric Strength | 14.7 kV/mm | 373 kV/in | Short Time; ASTM D149 |
Plenco 4100 Phenolic, Granular, Compression Molded
(discontinued **) Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and .. |
|||
Dielectric Strength | 14.7 kV/mm | 373 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance.. |
|||
Dielectric Strength | 14.7 kV/mm | 373 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 153 Phenolic, Compression Grade Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a.. |
|||
Dielectric Strength | 14.7 kV/mm | 373 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Dielectric Strength | 14.7 kV/mm | 373 kV/in | 60Hz, Short Time, dry; ASTM D149 |
Sumitomo Bakelite North America E 8354-19189-2 Electrical Encapsulation Grade Epoxy Glass and mineral reinforced epoxy molding compound, formulated for the encapsulation of devices requiring high quality and thermal shock resistance.Information provided by Vyncolit, a Sumitomo Bak .. |
|||
Dielectric Strength | 14.7 kV/mm | 373 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Dielectric Strength | 14.7 kV/mm | 373 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Dielectric Strength | 14.7 kV/mm | 373 kV/in | Short Time; ASTM D149 |
Plenco 6401 Phenolic, Granular, Compression Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |