Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total Lacqrene® 1240 Crystal Polystyrene
(discontinued **) LACQRENE® 1240 is a high molecular weight crystal polystyrene, used in the dilution of high impact grades of polystyrene such as LACQRENE® 7240 or clear impact polystyrene such as Finaclear 520. .. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total Lacqrene® 1250 Crystal Polystyrene
(discontinued **) LACQRENE® 1250 is a very high molecular weight crystal polystyrene mainly for the injection molding industry. It is characterized by a very good compromise between molecular weight, heat resistanc.. |
|||
Dielectric Strength | 135 kV/mm @Frequency 50.0 Hz, Temperature 150 °C |
3430 kV/in @Frequency 50.0 Hz, Temperature 302 °F |
DIN 40634 or VDE 0345 in air |
Mitsubishi Hostaphan® RN, 190 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Dielectric Strength | 135 kV/mm @Frequency 50.0 Hz, Temperature 150 °C |
3430 kV/in @Frequency 50.0 Hz, Temperature 302 °F |
DIN 40634 or VDE 0345 in air or ASTM D149 |
Mitsubishi Hostaphan® WN, 190 micron Nominal Thickness Translucent White Polyethylene Terephthalate Film Hostaphan® WN is a white film made of polyethylene terephthalate (PET) and is well suited for electrical insulating of machines and appliances. The high dielectric strength and large volume resis.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | K20/P50; IEC 60243-1 |
Styrolution Polystyrol 143 E GR 2 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | K20/P50; IEC 60243-1 |
Styrolution Polystyrol 143 E GR 21 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | K20/P50; IEC 60243-1 |
Styrolution Polystyrol 145 D PS Description: Polystyrol 145 D is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol.Applications: In blends with high impact polystyrene esp.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | K20/P50; IEC 60243-1 |
Styrolution Polystyrol 158 K GR 2 PS Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | K20/P50; IEC 60243-1 |
Styrolution Polystyrol 158 K GR 21 PS Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | K20/P50; IEC 60243-1 |
Styrolution Polystyrol 165 H GR 2 PS Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermo.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | K20/P50; IEC 60243-1 |
Styrolution Polystyrol 168 N GR 2 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | K20/P50; IEC 60243-1 |
Styrolution Polystyrol 168 N GR 21 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Dielectric Strength | 135 kV/mm @Thickness 1.50 mm |
3430 kV/in @Thickness 0.0591 in |
Short Time; IEC 60243-1 |
Styrolution PS 147F GPPS Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro.. |
|||
Dielectric Strength | 135 kV/mm @Thickness 1.50 mm |
3430 kV/in @Thickness 0.0591 in |
Short Time; IEC 60243-1 |
Styrolution PS 168N GPPS Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend componen.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | K20/P20; IEC 60243-1 |
Styrolution PS-145D Polystyrene Description: Polystyrene 145D is a high flow, general purpose polystyrene. PS 145D offers exceptional processing characteristics for thing walled parts, multi-cavity tools, and complex designs. It i.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | K20/P50; IEC 60243-1 |
Styrolution Polystyrol 165 H GR 21 PS Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermo.. |
|||
Dielectric Strength | 135 kV/mm @Thickness 1.50 mm |
3430 kV/in @Thickness 0.0591 in |
Short Time; IEC 60243-1 |
Styrolution PS 158K GPPS Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total PSC 1340 Crystal Polystyrene 1340 is a high molecular weight crystal polystyrene which allows maximum dilution rates with high impact polystyrene grades such as LACQRENE® 7240. In dilution, LACQRENE® 1340 gives excellent pro.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | ASTM D149 |
Total PSC 1450 High Heat Resistance, Easy Flow Crystal Polystyrene Total Petrochemicals Polystyrene 1450 is a high heat resistance, easy flow crystal polystyrene for injection molding and the foam extrusion industry. This product offers optimum fluidity and excell.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total PSC 1450N High Heat Resistance Polystyrene 1450N is a high heat resistance, easy flowing crystal polystyrene for the production of thick insulation board. The low viscosity of this grade makes it particularly suitable for the production of .. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total PSC 1540(EU) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total PSC 1960N Crystal Polystyrene 1960N is a high resistance crystal polystyrene with very high flow for the production of thick insulation board. The very low viscosity of this grade makes it particularly suitable for the producti.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total PSC 1160/1160N Crystal Polystyrene 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. Most notable for the production of bi-oriented polystyrene (BOPS). It is particularly useful.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total PSC 1540(AS) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total PSC 1810/1811 Polystyrene 1811 is a very easy flowing crystal polystyrene designed, principally, for the injection molding industry. The excellent processing characteristics of this grade allows for the production of articl.. |
|||
Dielectric Strength | 135 kV/mm | 3430 kV/in | |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |