Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.0 kV/mm | 482 kV/in | ASTM D149 |
Arlon 56596R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red si.. |