Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.5 kV/mm | 394 kV/in | Short Time; ASTM D149 |
Plenco 50240 PET, Pellet, Injection Molded, Blue
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |
|||
Dielectric Strength | 15.5 kV/mm | 394 kV/in | Short Time; ASTM D149 |
Plenco 2300 Phenolic, Granular, Compression Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Dielectric Strength | 15.5 kV/mm | 394 kV/in | Short time, 500 V/sec rate-of-rise; ASTM D149 |
Eastman Cadence™ GS4 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Dielectric Strength | 15.5 kV/mm | 394 kV/in | ASTM D149-97a |
DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12120 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12120 have a cherry-red appearance which tur.. |
|||
Dielectric Strength | 15.5 kV/mm | 394 kV/in | Short Time; ASTM D149 |
Plenco 1510 Polyester, Granular, Transfer Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |