Material Notes:
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 122.2 MPa
17720 psi
ASTM D638
Elongation at Break 1.68 %
1.68 %
ASTM D638
Tensile Modulus 12.53 GPa
1817 ksi
ASTM D638
Flexural Yield Strength 178.1 MPa
25830 psi
ASTM D790
Flexural Modulus 11.11 GPa
1611 ksi
ASTM D790
Compressive Yield Strength 154.9 MPa
22470 psi
ASTM D695
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 227 °C
441 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.10e+16 ohm-cm
1.10e+16 ohm-cm
ASTM D257
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.5 kV/mm
394 kV/in
Short Time; ASTM D149
Dissipation Factor 0.013

@Frequency 1e+6 Hz
0.013

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 40 sec
40 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638