Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 1.00e+13 - 1.00e+13 ohm @Temperature 90.0 - 90.0 °C |
1.00e+13 - 1.00e+13 ohm @Temperature 194 - 194 °F |
Average value: 1.00e+13 ohm Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Insulation Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | |
Gwent Electronic Materials D2121102P1 UV Curable Dielectric Ink Screen printable UV cured green dielectric ink with good printability and excellent flexibility. Provides excellent screen life and is suitable for use with automated reel to reel, semi-automatic or.. |
|||
Insulation Resistance | 1.00e+13 ohm @Temperature 90.0 °C |
1.00e+13 ohm @Temperature 194 °F |
IEC 60167 |
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi.. |
|||
Insulation Resistance | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | Dry; IEC 167 |
Vyncolit X655 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask.. |
|||
Insulation Resistance | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | Dry; IEC 167 |
Vyncolit X680 Novolac Phenolic Glass fiber and glass bead filled phenolic molding compound with excellent mechanical and thermal properties. Easily transformed into complex shapes. UL listed.USES: Complex precision parts with t.. |
|||
Insulation Resistance | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | Dry; IEC 167 |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |
|||
Insulation Resistance | 1.00e+13 ohm | 1.00e+13 ohm | 100VDC, 60 sec; Mil-I-46058C |
3M 7945MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Insulation Resistance | 1.00e+13 ohm | 1.00e+13 ohm | 100VDC, 60 sec; Mil-I-46058C |
3M 9045MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |