Vyncolit X681 Novolac Phenolic

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Vyncolit N.V., Sumitomo Bakelite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vyncolit X681 Novolac Phenolic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubricating bearings.Information provided by Vyncolit, a Sumitomo Bak Group
Physical Properties Metric English Comments
Bulk Density 0.700 - 0.850 g/cc
0.0253 - 0.0307 lb/in³
Powder Density; ISO 60
Density 1.70 g/cc
0.0614 lb/in³
Relative Density; ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
Injection Molding; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 - 60.0 MPa
7250 - 8700 psi
ISO 527
Elongation at Break 0.60 - 0.70 %
0.60 - 0.70 %
Tensile; ISO 527
1.3 - 1.4 %
1.3 - 1.4 %
Flexure; ISO 178
Tensile Modulus 9.50 - 11.5 GPa
1380 - 1670 ksi
ISO 527
Flexural Strength 130 - 150 MPa
18900 - 21800 psi
At Rupture; ISO 178
Flexural Modulus 9.00 - 11.0 GPa
1310 - 1600 ksi
ISO 178
Compressive Strength 220 - 240 MPa
31900 - 34800 psi
ISO 604
Charpy Impact Unnotched 0.750 - 0.900 J/cm²
3.57 - 4.28 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.250 - 0.400 J/cm²
1.19 - 1.90 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
22.2 - 27.8 µin/in-°F

@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 170 - 190 °C
338 - 374 °F
ISO 75 Af
Deflection Temperature at 8.0 MPa 150 - 170 °C
302 - 338 °F
ISO 75 C
Shrinkage 0.15 - 0.30 %
0.15 - 0.30 %
Post Shrinkage; ISO 2577
Electrical Properties Metric English Comments
Insulation Resistance 1.00e+13 - 1.00e+14 ohm
1.00e+13 - 1.00e+14 ohm
Dry; IEC 167
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 243
Comparative Tracking Index 175 V
175 V
IEC 112
Descriptive Properties Value Comments
Color Black
ISO type PF 2 C3
Main Filler Glass Fiber
Molding Method Compression, transfer, injection