Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vyncolit X680 Novolac Phenolic

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Vyncolit N.V., Sumitomo Bakelite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vyncolit X680 Novolac Phenolic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber and glass bead filled phenolic molding compound with excellent mechanical and thermal properties. Easily transformed into complex shapes. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. insulators, spacers, edge connectors, coil former, timer parts and computer componentsInformation provided by Vyncolit, a Sumitomo Bak Group
Physical Properties Metric English Comments
Bulk Density 0.650 g/cc
0.0235 lb/in³
Powder Density; ISO 60
Density 1.68 g/cc
0.0607 lb/in³
Relative Density; ISO 1183
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
Injection Molding; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa
10900 psi
ISO 527
Elongation at Break 0.65 %
0.65 %
Tensile; ISO 527
1.6 %
1.6 %
Flexure; ISO 178
Tensile Modulus 13.5 GPa
1960 ksi
ISO 527
Flexural Strength 190 MPa
27600 psi
At Rupture; ISO 178
Flexural Modulus 13.0 GPa
1890 ksi
ISO 178
Compressive Strength 280 MPa
40600 psi
ISO 604
Charpy Impact Unnotched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75 Af
Flammability, UL94 V-1

@Thickness 1.60 mm
V-1

@Thickness 0.0630 in
V-0

@Thickness 4.00 mm
V-0

@Thickness 0.157 in
Shrinkage 0.10 %
0.10 %
Post Shrinkage; ISO 2577
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
DIN 53482
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 93
Insulation Resistance 1.00e+11 ohm
1.00e+11 ohm
Wet; 24 hours in water; IEC 167
1.00e+13 - 1.00e+14 ohm
1.00e+13 - 1.00e+14 ohm
Dry; IEC 167
Dielectric Strength 20.0 kV/mm
508 kV/in
IEC 243
Comparative Tracking Index 125 V
125 V
IEC 112
Descriptive Properties Value Comments
Color Black, Green
ISO type PF 2 C1
Main Filler Glass Fiber & Glass Bead
Molding Method Compression, transfer, injection
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved