Polymer Property : Shielding Effectiveness = 80 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 80 - 100 dB
80 - 100 dB
modified specimen 0.85 mm x 1.0 mm bead with plastic bolts; MIL-G-83528 Para. 4.6.12
Parker Chomerics CHO-FORM® 5518 Robotically Dispensed Gasketing
Description: CHO-FORM® 5518 Two-component, thermal cure silicone system with Ag/Cu particle filler. Minimum cure temperature is only 85°C (185°F). Formulated for painted, plated or metalized plas..
Shielding Effectiveness >= 80 dB

@Frequency 1.00e+10 Hz
>= 80 dB

@Frequency 1.00e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer
Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R..
Shielding Effectiveness >= 80 dB
>= 80 dB
10 GHz (Plane Wave); MIL-G-83528
Parker Chomerics CHO-SEAL 1485 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Shielding Effectiveness >= 80 dB
>= 80 dB
10 GHz (Plane Wave); MIL-G-83528
Parker Chomerics CHO-SEAL 1501 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Shielding Effectiveness >= 80 dB
>= 80 dB
100 MHz (E Field); MIL-G-83528
Parker Chomerics CHO-SEAL 6309 Extruded Elastomer
Commercial Grade Extruded Elastomer. This is an extruded nickel-plated graphite filled silicone elastomer that provides a minimum shielding effectiveness of 75 dB from 100 MHz to 10 GHz. This low co..
Shielding Effectiveness >= 80 dB
>= 80 dB
500 MHz (E Field); MIL-G-83528
Parker Chomerics CHO-SEAL 6309 Extruded Elastomer
Commercial Grade Extruded Elastomer. This is an extruded nickel-plated graphite filled silicone elastomer that provides a minimum shielding effectiveness of 75 dB from 100 MHz to 10 GHz. This low co..
Shielding Effectiveness >= 80 dB
>= 80 dB
2 GHz (Plane Wave); MIL-G-83528
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer
Low Cost Commercial Grade Extruded Elastomer. CHO-SEAL 6310 is the latest addition to Chomerics line of low cost, commercial grade EMI gaskets. This extruded material combines nickel-plated graphite..
Shielding Effectiveness >= 80 dB
>= 80 dB
10 GHz (Plane Wave); MIL-G-83528
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer
Low Cost Commercial Grade Extruded Elastomer. CHO-SEAL 6310 is the latest addition to Chomerics line of low cost, commercial grade EMI gaskets. This extruded material combines nickel-plated graphite..
Shielding Effectiveness >= 80 dB
>= 80 dB
500 MHz (E Field); MIL-G-83528
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..
Shielding Effectiveness >= 80 dB
>= 80 dB
2 GHz (Plane Wave); MIL-G-83528
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..
Shielding Effectiveness >= 80 dB
>= 80 dB
10 GHz (Plane Wave); MIL-G-83528
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..
Shielding Effectiveness >= 80 dB
>= 80 dB
100 MHz (E Field); MIL-G-83528
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..
Shielding Effectiveness >= 80 dB

@Frequency 2.00e+9 Hz
>= 80 dB

@Frequency 2.00e+9 Hz
CHO-TM-TP08
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C..
Shielding Effectiveness >= 80 dB

@Frequency 1.00e+9 Hz
>= 80 dB

@Frequency 1.00e+9 Hz
CHO-TM-TP08
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C..