Low Cost Commercial Grade Extruded Elastomer. CHO-SEAL 6310 is the latest addition to Chomerics line of low cost, commercial grade EMI gaskets. This extruded material combines nickel-plated graphite filler in a silicone elastomer binder to offer high shielding effectiveness and a desirable price-performance balance.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 70
50 - 70
ASTM D2240
Tensile Strength at Break >= 0.689 MPa
>= 100 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Compression Set 35 %
35 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.10 ohm-cm
0.10 ohm-cm
without pressure-sensitive adhesive; CEPS-0002
<= 0.25 ohm-cm
<= 0.25 ohm-cm
After heat aging; CEPS-0002
Shielding Effectiveness >= 80 dB
>= 80 dB
2 GHz (Plane Wave); MIL-G-83528
>= 80 dB
>= 80 dB
10 GHz (Plane Wave); MIL-G-83528
>= 100 dB
>= 100 dB
100 MHz (E Field); MIL-G-83528
>= 100 dB
>= 100 dB
500 MHz (E Field); MIL-G-83528
Descriptive Properties Value Comments
Binder Silicone
Filler Ni/C