Material Notes:
Molding grade conductive EPDM elastomer loaded with nickel graphite filler. The material is dark grey in color and is specially compounded to give high EMC performance and excellent IP sealing.Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 95
85 - 95
ASTM D2240
Tensile Strength >= 1.60 MPa
>= 232 psi
ASTM D412
Elongation at Break >= 90 %
>= 90 %
ASTM D412
Compression Set <= 40 %

@Temperature 100 °C,
Time 259000 sec
<= 40 %

@Temperature 212 °F,
Time 72.0 hour
ASTM D395
Electrical Properties Metric English Comments
Volume Resistivity <= 0.50 ohm-cm
<= 0.50 ohm-cm
Mil-G-83528/MIL std 285
Shielding Effectiveness 85 dB

@Frequency 2.00e+9 Hz
85 dB

@Frequency 2.00e+9 Hz
Plane Wave; Mil-G-83528/MIL std 285
85 dB

@Frequency 1.00e+10 Hz
85 dB

@Frequency 1.00e+10 Hz
Plane Wave; Mil-G-83528/MIL std 285
90 dB

@Frequency 5.00e+8 Hz
90 dB

@Frequency 5.00e+8 Hz
E-Field; Mil-G-83528/MIL std 285
95 dB

@Frequency 1.00e+8 Hz
95 dB

@Frequency 1.00e+8 Hz
H-Field; Mil-G-83528/MIL std 285