Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | 1.00 - 2.00 sec | 1.00 - 2.00 sec | Average value: 1.67 sec Grade Count:3 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Static Decay | 1.00 - 2.00 sec | 1.00 - 2.00 sec | Average value: 1.80 sec Grade Count:10 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Static Decay | 1.00 sec | 1.00 sec | Average value: 1.00 sec Grade Count:4 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Static Decay | 1.00 sec | 1.00 sec | Average value: 1.00 sec Grade Count:3 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Static Decay | 1.00 - 2.00 sec | 1.00 - 2.00 sec | Average value: 1.86 sec Grade Count:7 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |