Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 124 sec | 124 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N4000-7 SI® FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Arc Resistance | 124 sec | 124 sec | |
Pyrotek TS-82 Thermoset Electrical Insulation Product (Nema Grade: XXX) Paper reinforcement, Phenolic Resin, Natural Color. High humidity resistance, Excellent resistance to splitting.Information provided by Pyrotek. |
|||
Arc Resistance | 124 sec | 124 sec | ASTM D495 |
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Arc Resistance | 124 sec | 124 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N4000-7 FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Arc Resistance | 124 sec | 124 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N7000-2 V0 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 V0 series is a next-generation high-Tg polyimide using a toughened resin chemistry to achieve a UL 94-V0 designation. This advanced material is designed for use in a wide variety o.. |
|||
Arc Resistance | 124 sec @Thickness 3.17 mm |
124 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Arc Resistance | 124 sec | 124 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta.. |
|||
Arc Resistance | 124 sec | 124 sec | 23°C; ASTM D-495 |
UBE UPIMOL® R Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |
|||
Arc Resistance | 124 sec | 124 sec | ASTM D495 |
Eastman TiGlaze SV Copolyester TiGLAZE SV copolyester is a specialty copolyester for the architectural glazing industry, designed to provide a unique balance of toughness, stiffness and material value. The material has a CC1 Ligh.. |
|||
Arc Resistance | 124 sec | 124 sec | |
Dow Corning 111 VALVE LUBRICANT & SEALANT General purpose O-ring and valve lubricant. Provides a noncuring moisture barrier; high dielectric strength; moisture and ozone resistance; good thermal, oxidation and chemical stability; suitable .. |
|||
Arc Resistance | 124 sec | 124 sec | IPC TM-650 2.5.1 |
Arlon 37N Polyimide Low-Flow 37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir.. |
|||
Arc Resistance | 124 sec | 124 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
Arc Resistance | 124 sec | 124 sec | ASTM D495 |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |