Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman TiGlaze SV Copolyester

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name TiGlaze
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman TiGlaze SV Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TiGLAZE SV copolyester is a specialty copolyester for the architectural glazing industry, designed to provide a unique balance of toughness, stiffness and material value. The material has a CC1 Light Transmitting Plastic Rating and, in sheet form, will pass UL972 for Burglary Resistant Glazing. Sheet produced from TiGLAZE SV copolyester is coextruded with a UV layer to offer protection from damaging UV rays. TiGLAZE SV copolyester is used in skylights, barrel vaults and flat glazing applications.The material failed to discharge under a Static Decay Rate test ASTM D4470.Applications/UsesArchitectural glazingFlat and sloped glazingKiosksSkylightsWaiting shelters
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Water Absorption 0.16 %
0.16 %
24h Immersion; ASTM D570
Thickness 3000 microns
118 mil
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D638
Tensile Strength, Yield 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 156 %
156 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 2.30 GPa
334 ksi
ASTM D638
Flexural Yield Strength 82.0 MPa
11900 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 0.340 J/cm

@Temperature -30.0 °C
0.637 ft-lb/in

@Temperature -22.0 °F
ASTM D256
>= 0.540 J/cm

@Temperature 0.000 °C
>= 1.01 ft-lb/in

@Temperature 32.0 °F
ASTM D256
0.600 J/cm

@Temperature 23.0 °C
1.12 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ASTM D4812
Puncture Energy 33.0 J
24.3 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
35.0 J
25.8 ft-lb
Puncture Resistance @Max Load, -30°C; ASTM D3763
39.0 J
28.8 ft-lb
Puncture Resistance @Max Load, -10°C; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 7.00 µm/m-°C

@Temperature 20.0 °C
3.89 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
ASTM D648
Vicat Softening Point 80.0 °C
176 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 2.8 %
2.8 %
ASTM D1003
Gloss 148 %
148 %
at 60°; ASTM D2457
Transmission, Visible 88 %
88 %
Total Transmittance; ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Surface Resistivity per Square 1.00e+17 ohm
1.00e+17 ohm
ASTM D257
Arc Resistance 124 sec
124 sec
ASTM D495
Descriptive Properties Value Comments
Color, CIE a* -0.1
VGAS-A-AN-G-RS-001
Color, CIE b* 1.92
VGAS-A-AN-G-RS-001
Color, CIE L* 93.3
VGAS-A-AN-G-RS-001
Copyright © lookpolymers.com All Rights Reserved