Electrical Properties Metric English Comments
Arc Resistance 105 sec
105 sec
Practical Use (Water Absorption 3.5%); ASTM-D495
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Arc Resistance 105 sec
105 sec
Practical Use (Water Absorption 3.0%); ASTM-D495
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Arc Resistance 105 sec
105 sec
Practical Use (Water Absorption 3.5%); ASTM-D495
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..