Electrical Properties Metric English Comments
Surface Resistivity per Square 30000 ohm
30000 ohm
ASTM D257
Ovation Polymers Nemcon™ E-PC CB Polycarbonate
Nemcon E-series products are designed for use in ESDA electronic assembly environments. Nemcon E-PC CB is a carbon black-filled polycarbonate characterized by consistent moldability, recyclability,..
Surface Resistivity per Square 30000 - 1.40e+7 ohm
30000 - 1.40e+7 ohm
Panipol Oy W Dispersions Inherently Conductive Polymer
Doped polyaniline as water dispersionSolution Processing, Coating formulations, Ink formulationsInformation provided by Panipol Oy Ltd