Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 30000 ohm | 30000 ohm | ASTM D257 |
Ovation Polymers Nemcon™ E-PC CB Polycarbonate Nemcon E-series products are designed for use in ESDA electronic assembly environments. Nemcon E-PC CB is a carbon black-filled polycarbonate characterized by consistent moldability, recyclability,.. |
|||
Surface Resistivity per Square | 30000 - 1.40e+7 ohm | 30000 - 1.40e+7 ohm | |
Panipol Oy W Dispersions Inherently Conductive Polymer Doped polyaniline as water dispersionSolution Processing, Coating formulations, Ink formulationsInformation provided by Panipol Oy Ltd |