Ovation Polymers Nemcon™ E-PC CB Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Ovation Polymers
Trade Name Nemcon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nemcon™ E-PC CB Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nemcon E-series products are designed for use in ESDA electronic assembly environments. Nemcon E-PC CB is a carbon black-filled polycarbonate characterized by consistent moldability, recyclability, low outgassing, and good conductivity. ApplicationsShipping/handling trays for components, ICs and circuit assembliesInternal components/assembliesInformation provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.0 MPa
8990 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 63.0 MPa
9140 psi
50 mm/min; ASTM D638
Elongation at Break 14 %
14 %
50 mm/min; ASTM D638
Tensile Modulus 2.78 GPa
403 ksi
50 mm/min; ASTM D638
Flexural Strength 100 MPa
14500 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.561 J/cm

@Temperature 23.0 °C
1.05 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C

@Thickness 3.20 mm
266 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 30000 ohm
30000 ohm
ASTM D257