Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Panipol Oy W Dispersions Inherently Conductive Polymer

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Panipol
Trade Name Oy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Panipol Oy W Dispersions Inherently Conductive Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Doped polyaniline as water dispersionSolution Processing, Coating formulations, Ink formulationsInformation provided by Panipol Oy Ltd
Physical Properties Metric English Comments
Solids Content 6.0 %
6.0 %
pH 2.0 - 3.0
2.0 - 3.0
Viscosity 18000 cP
18000 cP
Thermal Properties Metric English Comments
Decomposition Temperature 250 °C
482 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square 30000 - 1.40e+7 ohm
30000 - 1.40e+7 ohm
Descriptive Properties Value Comments
CAS Number 15996-80-2
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved