Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total Lacqrene® 1250 Crystal Polystyrene
(discontinued **) LACQRENE® 1250 is a very high molecular weight crystal polystyrene mainly for the injection molding industry. It is characterized by a very good compromise between molecular weight, heat resistanc.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total Lacqrene® 3351(AS) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | VDE 0303 |
GEHR Plastics PET Polyethylene Terephthalate Polyethylene terephthalate shows high tensile and mechanical strength, hardness and toughness, low friction and a high dimensional stability. PET may be used at temperatures ranging from -20°C to.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | VDE 0303 |
GEHR Plastics POM-10PE Acetal Copolymer Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | VDE 0303 |
GEHR Plastics PVDF Polyvinylidene Fluoride Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan.. |
|||
Surface Resistivity per Square | 1.00e+14 ohm @Temperature 23.0 °C |
1.00e+14 ohm @Temperature 73.4 °F |
50% RH; ASTM D250 |
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total PSC 1450N High Heat Resistance Polystyrene 1450N is a high heat resistance, easy flowing crystal polystyrene for the production of thick insulation board. The low viscosity of this grade makes it particularly suitable for the production of .. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total PSC 1540(AS) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Surface Resistivity per Square | 1.00e+14 ohm | 1.00e+14 ohm | |
Goodfellow Polyethylene Naphthalate (PEN) Film A polyester that is chemically quite similar to PET but which is more temperature resistant. So far available only as biaxially oriented and heat stabilized films, they are semi-crystalline and colo.. |
|||
Surface Resistivity per Square | 1.00e+14 ohm | 1.00e+14 ohm | |
Goodfellow Topas® Cyclo-olefin copolymer Information provided by Goodfellow. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm @Temperature 20.0 °C |
>= 1.00e+14 ohm @Temperature 68.0 °F |
500 V DC at 95% rh; ASTM D257-83 |
DuPont Teijin Films Melinex® 329 Polyester Film, 200 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | < 1V after 2 min - 500 V; ASTM D257 |
3M Dyneon™ PVDF 31508/0003 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 31508/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. PVDF 31508/0003 also has a very low brittleness temperature, for.. |