Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled

Category Polymer , Thermoplastic , Nylon
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.79 g/cc
1.79 g/cc
ASTM D792
Water Absorption 0.30 %

@Temperature 23.0 °C
0.30 %

@Temperature 73.4 °F
ASTM D570
Melt Flow 30 g/10 min

@Load 1.20 kg,
Temperature 300 °C
30 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.7 MPa
9530 psi
5 mm/min; ASTM D638
Flexural Strength 108 MPa
15700 psi
2.8 mm/min; ASTM D638
Flexural Modulus 6.08 GPa
882 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 0.392 J/cm

@Thickness 6.35 mm
0.735 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 247 °C

@Thickness 6.40 mm
477 °F

@Thickness 0.252 in
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+14 ohm

@Temperature 23.0 °C
1.00e+14 ohm

@Temperature 73.4 °F
50% RH; ASTM D250