Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

GEHR Plastics POM-10PE Acetal Copolymer

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer GEHR Plastics Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GEHR Plastics POM-10PE Acetal Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear because of the high strength and smooth surface. There is a very low risk of stress cracks. POM-C exhibits a high thermal stability and a high resistance to chemicals. Improved sliding properties for applications with increased abrasion.Properties:no microporosityhigh strengthhigh rigidityhigh thermal stabilitylow water absorptionhigh dimension stabilitygood electrical insulating propertiesvery good sliding propertieshigh resistance to stress cracksnot resistant to high concentrated acidsdifficult to glue and paintApplications include bearings, fittings, gear wheels, parts for pumps, screws, bobbins, parts for textile industry, and medium for coating lines.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ISO 1183
Water Absorption 0.20 %
0.20 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO 527
Modulus of Elasticity 2.20 GPa
319 ksi
ISO 527
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Maximum Service Temperature, Air 100 °C
212 °F
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
ISO 75
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
VDE 0303
Surface Resistivity per Square >= 1.00e+14 ohm
>= 1.00e+14 ohm
VDE 0303
Dielectric Constant 4.4

@Frequency 1.00e+6 Hz
4.4

@Frequency 1.00e+6 Hz
DIN 53483
Dielectric Loss Index 0.0030

@Frequency 1.00e+6 Hz
0.0030

@Frequency 1.00e+6 Hz
DIN 53483
Descriptive Properties Value Comments
Acid Resistance no
Bondability no
Color Light Blue
Users viewing this material also viewed the following: