Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir ICE R 830D Polystyrene Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir N 1782 Polystyrene General purpose polystyrene with good flow and high heat resistance. Suggested for direct gassing extrusion of heavy gage insulating boards (XPS) and in blend with high concentration of clear SBS f.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir N 1840 Polystyrene General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir N 2560 Polystyrene High molecular weight general purpose polystyrene with good mechanical strength and good thermal resistance. It is recommended for in-line forming of disposable packaging, for sheet
extrusion in ble.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir R 321P Polystyrene Medium impact polystyrene combining easy flow and high stiffness. For injection moulding of parts with low thickness and high rigidity. Designation: Thermoplastics ISO 2897-PS-I,M,083-12-04-30Applic.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir R 540E Polystyrene HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection
moldings. Designation: Thermoplastics IS.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir RK 451G Polystyrene UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded, high impact polystyrene. This grade combines medium flow, heat resistance and good light stability for injection moulding of technical p.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir RK 5512G Polystyrene UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal properties. It exhibits a good stability to the processing conditions and to the light
exposure.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir RT 441M Polystyrene High impact polystyrene combining high toughness and high stiffness with good flowability for easy processing. Designed for injection moulding of technical parts, housings and covers.
Especially rec.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir RT 461F Polystyrene High impact, heat resistant polystyrene with good stiffness. Recommended for improving the thermal performance of injection moulded technical parts which are submitted to high temperature in service.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Surface Resistance | >= 1.50e+15 ohm | >= 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir® PD ICE S 900 High Impact Polystyrene - Very High ESCR Very high environmental stress cracking resistant (VH ESCR) HIPS.ICE S 900 exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents, and in particular to cyclopent.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir N 2380 Polystyrene High molecular weight general purpose polystyrene combining high heat resistance and good mechanical strength. Suitable for direct gassing extrusion, for biaxially oriented films and sheets, for gla.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir RC 600 Polystyrene Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir RK Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir RKL Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is designed for the extrusion of flame retardant sheets, foils and profiles. Designation: Thermoplastics ISO 2897-PS-I,E,093-06-04-18App.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir ICE S 800/N Polystyrene
(discontinued **) Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t.. |
|||
Surface Resistance | 1.50e+15 ohm | 1.50e+15 ohm | IEC 60093 |
Polimeri Europa Edistir N 1910 Polystyrene Very easy flow general purpose polystyrene. Used for injection of thin-wall, multi-cavity, very fast-cycle mouldings and for sheet extrusion in glossy capping of HIPS and in blend with HIPS or clear.. |