Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 40000 V @Thickness 1.57 mm |
40000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP310E Cotton Fabric Description: Manufactured with a domestic cotton fabric and phenolic resin. Similar to NP310 with improved moisture resistance and electrical properties. Mechanical properties equivalent to NP310. M.. |
|||
Dielectric Breakdown | 40000 V @Thickness 1.57 mm |
40000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP629 Paper Base Laminate Description: It is a paper-phenolic high-pressure laminate. It is intended primarily for mechanical applications and is suitable for electrical applications as well. Thickness Tested: 0.062", 0.125".. |
|||
Dielectric Breakdown | 40000 V @Thickness 1.57 mm |
40000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP630 Paper Base Laminate Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Dielectric Breakdown | >= 40000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 40000 V @Temperature 194 °F, Time 0.00556 hour |
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe EP CC 31 Woven Cotton Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 40000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 40000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe EP CC 31 Woven Cotton Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 40000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 40000 V @Temperature 194 °F, Time 0.00556 hour |
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe EP GC 21 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relative .. |
|||
Dielectric Breakdown | >= 40000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 40000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe EP GC 21 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relative .. |
|||
Dielectric Breakdown | >= 40000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 40000 V @Temperature 194 °F, Time 0.00556 hour |
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe EP GC 22 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. High mechanical strength at elevated temperatures. Very good stability of .. |
|||
Dielectric Breakdown | >= 40000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 40000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe EP GC 22 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. High mechanical strength at elevated temperatures. Very good stability of .. |
|||
Dielectric Breakdown | >= 40000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 40000 V @Temperature 194 °F, Time 0.00556 hour |
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe EP GC 41 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. High mechanical strength at moderate temperatures. Good stability of electrical properties when exposed to high relative humidity.Inform.. |
|||
Dielectric Breakdown | >= 40000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 40000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe EP GC 41 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. High mechanical strength at moderate temperatures. Good stability of electrical properties when exposed to high relative humidity.Inform.. |