Description: It is a paper-phenolic high-pressure laminate. It is intended primarily for mechanical applications and is suitable for electrical applications as well. Thickness Tested: 0.062", 0.125" and 0.500"
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.40 g/cc

@Thickness 1.57 mm
1.30 - 1.40 g/cc

@Thickness 0.0620 in
ASTM D792
Moisture Absorption at Equilibrium 2.0 %

@Thickness 1.57 mm
2.0 %

@Thickness 0.0620 in
ASTM D229
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85 - 105

@Thickness 1.57 mm
85 - 105

@Thickness 0.0620 in
ASTM D785
Tensile Strength, Yield 79.3 MPa

@Thickness 1.57 mm
11500 psi

@Thickness 0.0620 in
CW; ASTM D638
93.1 MPa

@Thickness 1.57 mm
13500 psi

@Thickness 0.0620 in
LW; ASTM D638
Flexural Strength 117 MPa

@Thickness 1.57 mm
17000 psi

@Thickness 0.0620 in
CW; ASTM D790
152 MPa

@Thickness 1.57 mm
22000 psi

@Thickness 0.0620 in
LW; ASTM D790
Compressive Strength 172 MPa

@Thickness 12.7 mm
25000 psi

@Thickness 0.500 in
ASTM D695
Shear Strength 79.3 MPa

@Thickness 15.7 mm
11500 psi

@Thickness 0.620 in
ASTM D732
Izod Impact, Unnotched 0.214 J/cm

@Thickness 12.7 mm
0.400 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
0.267 J/cm

@Thickness 12.7 mm
0.500 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.57 mm
HB

@Thickness 0.0620 in
Electrical Properties Metric English Comments
Dielectric Constant 6.2

@Thickness 1.57 mm
6.2

@Thickness 0.0620 in
Permittivity, Cond D-24/23; ASTM D150
Dielectric Breakdown 5000 V

@Thickness 1.57 mm
5000 V

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S/S
40000 V

@Thickness 1.57 mm
40000 V

@Thickness 0.0620 in
Cond A; ASTM D229 S/S
Dissipation Factor 0.052

@Thickness 1.57 mm
0.052

@Thickness 0.0620 in
Cond D-24/23; ASTM D150
Descriptive Properties Value Comments
Bond Strength 900 lb
0.5", ASTM D229
Color Natural, Black
Users viewing this material also viewed the following: