Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hippe EP CC 31 Woven Cotton Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod

Category Polymer , Thermoset , Epoxy
Manufacturer Erhard Hippe KG
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe EP CC 31 Woven Cotton Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in mechanical, electrical and electronic applications.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.40 g/cc
1.20 - 1.40 g/cc
IEC 1212-2 7.2
Mechanical Properties Metric English Comments
Compressive Strength >= 125 MPa
>= 18100 psi
Axial; IEC 1212-2 4.2
Electrical Properties Metric English Comments
Insulation Resistance >= 7.50e+7 ohm

@Diameter 8.00 - 10.0 mm
>= 7.50e+7 ohm

@Diameter 0.315 - 0.394 in
After immersion in water; IEC 1212-2 5.2
Dielectric Constant <= 6.0

@Frequency 48.0 - 62.0 Hz
<= 6.0

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 5.3
<= 6.0

@Frequency 1.00e+6 Hz
<= 6.0

@Frequency 1.00e+6 Hz
IEC 1212-2 5.3
Dielectric Breakdown >= 40000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 40000 V

@Temperature 194 °F,
Time 0.00556 hour
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
>= 40000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 40000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Dissipation Factor <= 0.050

@Frequency 48.0 - 62.0 Hz
<= 0.050

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 5.3
<= 0.050

@Frequency 1.00e+6 Hz
<= 0.050

@Frequency 1.00e+6 Hz
IEC 1212-2 5.3
Descriptive Properties Value Comments
Cohesion between layers > 100 MPa
IEC 1212-2 4.3, Internal diameter <100 mm
Thermal Endurance 130 T.I.
IEC 1212-2 7.1
Water Absorption < 3 mg/cm²
IEC 1212-2 7.1
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved