Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 50000 ohm-cm | 50000 ohm-cm | specific resistance |
Imerys Kaolexâ„¢ BN Kaolin Kaolex BN is a Hydrated Aluminum Silicate. It is an econoMical high surface area clay, well suited for use in roofing granules and refractory applications..Information provided by Imerys |
|||
Electrical Resistivity | 50000 - 300000 ohm-cm | 50000 - 300000 ohm-cm | |
Heraeus Cleviosâ„¢ P VP CH 8000 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P VP CH 8000 is an antistatic material based o.. |
|||
Electrical Resistivity | 50000 ohm-cm | 50000 ohm-cm | Average |
Shakespeare Sanstat® CN125 .21mm Nylon 66 Monofilament Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by .. |
|||
Electrical Resistivity | 50000 ohm-cm @Temperature 500 °C |
50000 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 50000 ohm-cm | 50000 ohm-cm | |
BASF Theroplast® Red 454 Color Additive Chemical Structure: Monoazo RedApplication: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BA.. |
|||
Electrical Resistivity | 50000 ohm-cm | 50000 ohm-cm | |
BASF Theroplast® Black X70 Color Additive Application: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, PA and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BASF |