Material Notes:
Application: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, PA and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.300 g/cc
0.0108 lb/in³
Density 1.40 g/cc
0.0506 lb/in³
pH 6.0 - 7.0
6.0 - 7.0
Specific Surface Area 2.0 m²/g
2.0 m²/g
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Electrical Properties Metric English Comments
Electrical Resistivity 50000 ohm-cm
50000 ohm-cm
Descriptive Properties Value Comments
Color Black
Light Fastness 8