BASF Theroplast® Red 454 Color Additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BASF
Trade Name Theroplast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Theroplast® Red 454 Color Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Structure: Monoazo RedApplication: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.160 g/cc
0.00578 lb/in³
Density 1.30 g/cc
0.0470 lb/in³
pH 4.0 - 5.0
4.0 - 5.0
Specific Surface Area 2.0 m²/g
2.0 m²/g
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Electrical Properties Metric English Comments
Electrical Resistivity 50000 ohm-cm
50000 ohm-cm
Descriptive Properties Value Comments
Color Red
Light Fastness 8