Material Notes:
Kaolex BN is a Hydrated Aluminum Silicate. It is an econoMical high surface area clay, well suited for use in roofing granules and refractory applications..Information provided by Imerys
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Brightness 70 - 80 %
70 - 80 %
% Reflectance
Particle Size 0.30 µm
0.30 µm
average
Particle Mesh Size 325 Mesh
325 Mesh
0.4% retained
pH 4.5 - 5.5
4.5 - 5.5
Specific Surface Area 33 - 38 m²/g
33 - 38 m²/g
Brookfield Viscosity 500 - 1000 cP

@Temperature 25.0 - 500 °C
500 - 1000 cP

@Temperature 77.0 - 932 °F
20 RPM, 70% clay/water slip
Electrical Properties Metric English Comments
Electrical Resistivity 50000 ohm-cm
50000 ohm-cm
specific resistance
Descriptive Properties Value Comments
Color white
Heating Loss (% max as produced) 1
at 105°C