Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+12 - 2.00e+14 ohm-cm | 1.00e+12 - 2.00e+14 ohm-cm | Average value: 1.99e+13 ohm-cm Grade Count:22 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Electrical Resistivity | 7.40e+13 - 2.00e+14 ohm-cm | 7.40e+13 - 2.00e+14 ohm-cm | Average value: 1.00e+14 ohm-cm Grade Count:5 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Electrical Resistivity | 10000 - 2.00e+14 ohm-cm | 10000 - 2.00e+14 ohm-cm | Average value: 5.91e+13 ohm-cm Grade Count:30 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |