Electrical Properties Metric English Comments
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
RT
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
RT
Outokumpu 4501 Duplex Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
RT
Outokumpu SAF 2304® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
RT
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Electrical Resistivity 0.0000800 ohm-cm - 1e+05
0.0000800 ohm-cm - 1e+05
Average value: 0.0736 ohm-cm Grade Count:105
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 - 100 °C
0.0000800 ohm-cm

@Temperature 68.0 - 212 °F
Industeel CLC 17.13.5 LN Modified 317LN Mo 4% Austenitic Stainless Steel
Description: CLC 17-13-5LN (317LNM) is a Nitrogen alloyed austenitic stainless steel with a high Molybdenum addition (=4%). Alloy CLC 17-13-5LN (317LNM) exhibits austenitic microstructure free of de..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 - 100 °C
0.0000800 ohm-cm

@Temperature 68.0 - 212 °F
Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition
Description: CLC 18-12-4LN (317LN) is a Nitrogen alloyed austenitic stainless steel with a 3% Mo minimum addition (>4%). Alloys CLC 18-12-4LN (317LN) exhibit austenitic microstructure free of delete..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel
Description: CLI SIRIUS 309 grade is a fully austenitic stainless steel containing 23% Cr, and 13% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance b..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness
Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24
Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F
Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34
Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F
Industeel URANUS® B6 N Multipurpose Austenitic Stainless Steel with PREN = 36
Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling)
Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi..
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
Special Metals INCOLOY® 25-6M0 Super Austenitic Stainless Steel (UNS N08926)
Data provided by the manufacturer, Special Metals.
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
Special Metals NILO® Alloy 36 Low-Expansion Alloy
Inflection point 220°C. A nickel-iron low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coeffic..
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
Martensitic
Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy
Shape memory alloy is a description applied to that group of metallic materials which show the ability to return to the previously defined shape or size when subjected to the correct thermal procedu..
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
Carlson 926 Mo Austenitic Stainless Steel
General DescriptionCarlson alloy 926 Mo is a “super-austenitic” 6% molybdenum stainless steel that provides excellent resistance to a variety of highly corrosive environments. This alloy performs..
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition A
AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34
Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion..
Electrical Resistivity 0.0000800 ohm-cm
0.0000800 ohm-cm
RT
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel
Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom..
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour + air cooled)
Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corrosio..