Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | RT |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | RT |
Outokumpu 4501 Duplex Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | RT |
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | RT |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm - 1e+05 | 0.0000800 ohm-cm - 1e+05 | Average value: 0.0736 ohm-cm Grade Count:105 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 - 100 °C |
0.0000800 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.13.5 LN Modified 317LN Mo 4% Austenitic Stainless Steel Description: CLC 17-13-5LN (317LNM) is a Nitrogen alloyed austenitic stainless steel with a high Molybdenum addition (=4%). Alloy CLC 17-13-5LN (317LNM) exhibits austenitic microstructure free of de.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 - 100 °C |
0.0000800 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition Description: CLC 18-12-4LN (317LN) is a Nitrogen alloyed austenitic stainless steel with a 3% Mo minimum addition (>4%). Alloys CLC 18-12-4LN (317LN) exhibit austenitic microstructure free of delete.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 °C |
0.0000800 ohm-cm @Temperature 68.0 °F |
|
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel Description: CLI SIRIUS 309 grade is a fully austenitic stainless steel containing 23% Cr, and 13% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance b.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 °C |
0.0000800 ohm-cm @Temperature 68.0 °F |
|
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 °C |
0.0000800 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24 Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 °C |
0.0000800 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34 Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 °C |
0.0000800 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® B6 N Multipurpose Austenitic Stainless Steel with PREN = 36 Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 °C |
0.0000800 ohm-cm @Temperature 68.0 °F |
|
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | |
Special Metals INCOLOY® 25-6M0 Super Austenitic Stainless Steel (UNS N08926) Data provided by the manufacturer, Special Metals. |
|||
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | |
Special Metals NILO® Alloy 36 Low-Expansion Alloy Inflection point 220°C. A nickel-iron low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coeffic.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | |
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | Martensitic |
Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy Shape memory alloy is a description applied to that group of metallic materials which show the ability to return to the previously defined shape or size when subjected to the correct thermal procedu.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | |
Carlson 926 Mo Austenitic Stainless Steel General DescriptionCarlson alloy 926 Mo is a “super-austenitic” 6% molybdenum stainless steel that provides excellent resistance to a variety of highly corrosive environments. This alloy performs.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition A AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 °C |
0.0000800 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34 Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | RT |
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 °C |
0.0000800 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom.. |
|||
Electrical Resistivity | 0.0000800 ohm-cm @Temperature 20.0 °C |
0.0000800 ohm-cm @Temperature 68.0 °F |
|
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour + air cooled) Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corrosio.. |