Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000360 ohm-cm | 0.00000360 ohm-cm | |
Hogen Durakut H15W 68 Tungsten/32 Copper PM Metal Composite RWMA Class ECM-EDMDURAKUT Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Che.. |
|||
Electrical Resistivity | 0.00000360 ohm-cm | 0.00000360 ohm-cm | |
Mi-Tech Metals CW70E 68 Tungsten/32 Copper PM Metal Composite RWMA Class ECM-EDMMi-Tech Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Che.. |
|||
Electrical Resistivity | 0.00000360 - 0.00000420 ohm-cm | 0.00000360 - 0.00000420 ohm-cm | Temper T651 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |
|||
Electrical Resistivity | 0.00000360 - 0.00000420 ohm-cm | 0.00000360 - 0.00000420 ohm-cm | Temper T651 |
Constellium PLAN 6082 Aluminum Rolled Plate Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Electrical Resistivity | 0.00000360 - 0.00000420 ohm-cm | 0.00000360 - 0.00000420 ohm-cm | temper T651 |
Constellium Planoxal® 60 Aluminum plate The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use.. |
|||
Electrical Resistivity | 0.00000360 - 0.00000420 ohm-cm | 0.00000360 - 0.00000420 ohm-cm | Temper T651 |
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |