Electrical Properties Metric English Comments
Electrical Resistivity 0.00000313 ohm-cm
0.00000313 ohm-cm
(55% IACS)
CMW® D55 Silver Cadmium Oxide Contact Material ASTM B781, Table 2, Type B
For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc.
Electrical Resistivity 0.00000313 ohm-cm
0.00000313 ohm-cm
(55% IACS)
CMW® D56 Silver Nickel Contact Material B693
For electrical contacts; resistant to mechanical wearInformation provided by CMW Inc.
Electrical Resistivity 0.00000313 ohm-cm
0.00000313 ohm-cm
(55% IACS)
CMW® D58 Silver Graphite Contact Material
For electrical contacts; resistant to sliding wear.Information provided by CMW Inc.
Electrical Resistivity 0.00000313 ohm-cm
0.00000313 ohm-cm
(55% IACS)
CMW® ELKONITE® 35S Silver Tungsten contact material ASTM B631, Class B, infiltrated
For arcing and current carrying electrical contacts; household and power circuit breakers.Information provided by CMW Inc.
Electrical Resistivity 0.00000313 - 0.00000417 ohm-cm
0.00000313 - 0.00000417 ohm-cm
ALIMEX PLANAL 6082 T651 Aluminum Alloy
Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi..
Electrical Resistivity 0.00000313 - 0.00000417 ohm-cm
0.00000313 - 0.00000417 ohm-cm
ALIMEX 6082 T651 Aluminum Alloy Rolled
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then artificially aged.