CMW® D55 Silver Cadmium Oxide Contact Material ASTM B781, Table 2, Type B

Category Metal , Metal Matrix Composite , Nonferrous Metal , Precious Metal , Silver Alloy
Manufacturer CMW Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® D55 Silver Cadmium Oxide Contact Material ASTM B781, Table 2, Type B.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc.
Physical Properties Metric English Comments
Density 9.59 g/cc
0.346 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell F 35
35
Tensile Strength, Ultimate 83.0 MPa
12000 psi
Thermal Properties Metric English Comments
Melting Point <= 980 °C
<= 1800 °F
Liquidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
CdO 15 %
15 %
Silver, Ag 85 %
85 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000313 ohm-cm
0.00000313 ohm-cm
(55% IACS)