Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Lubricomp® LCL-4033 EM Polyetheretherketone, Carbon Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Lubricomp® LL-4040 Polyetheretherketone, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Stat-Kon® LCL-4026 EM BK8-115 Polyetheretherketone, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(d Features: Electrically Conductive, Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discont.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Thermocomp® LC-1006 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Thermocomp® LF-1003 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Thermocomp® LF-1004 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Thermocomp® LF-1006 EM Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Melt Temperature | 379 - 388 °C | 714 - 730 °F | |
LNP Thermocomp® LF-1006 MG Polyetheretherketone, Glass milled Glass Fiber
(discontinued **) Features: Low WarpageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still a.. |