Polymer Property : Melt Temperature = 624 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 321 - 329 °C
610 - 624 °F
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better ..
Melt Temperature 316 - 329 °C
601 - 624 °F
LNP Lubricomp® UFL-4036 HS Polyphthalamide, Glass Fiber Reinforced, PTFE Lubricant  (discontinued **)
Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr..
Melt Temperature 316 - 329 °C
601 - 624 °F
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Melt Temperature 316 - 329 °C
601 - 624 °F
LNP Thermocomp® UF-1006 HS Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..
Melt Temperature 316 - 329 °C
601 - 624 °F
LNP Thermocomp® UF-1009 HS Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Melt Temperature 321 - 329 °C
610 - 624 °F
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet..
Melt Temperature 321 - 329 °C
610 - 624 °F
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet..
Melt Temperature 316 - 329 °C
601 - 624 °F
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr..
Melt Temperature 316 - 329 °C
601 - 624 °F
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..
Melt Temperature 316 - 329 °C
601 - 624 °F
LNP Thermocomp® UF-1008 Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Melt Temperature 316 - 329 °C
601 - 624 °F
LNP Thermocomp® UFM-3249 HS BK8-115 Polyphthalamide, Glass Mineral Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..
Melt Temperature 316 - 329 °C
601 - 624 °F
LNP Verton™ UF-700-10 Polyphthalamide, Long Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..