LNP Verton™ UF-700-10 Polyphthalamide, Long Glass Fiber Reinforcement  (discontinued **)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LNP Verton™ UF-700-10 Polyphthalamide, Long Glass Fiber Reinforcement  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.
Physical Properties Metric English Comments
Specific Gravity 1.63 g/cc
1.63 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 245 MPa
35500 psi
ISO 527-1, -2
Elongation at Break 1.5 %
1.5 %
ISO 527-1, -2
Tensile Modulus 20.4 GPa
2960 ksi
ISO 527-1, -2
Flexural Strength 360 MPa
52200 psi
ISO 178
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
Processing Properties Metric English Comments
Melt Temperature 316 - 329 °C
601 - 624 °F
Mold Temperature 135 - 163 °C
275 - 325 °F
Drying Temperature 121 - 149 °C
250 - 300 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Suggested
Back Pressure 0.172 - 0.345 MPa
24.9 - 50.0 psi