Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 304 - 332 °C | 579 - 630 °F | |
PolyOne LubriOne™ PC-20CF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 316 - 332 °C | 601 - 630 °F | |
PolyOne LubriOne™ SF2-30CF/15T Natural Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 304 - 332 °C | 579 - 630 °F | |
PolyOne Therma-Tech™ SF-4500 TC Polyphenylene Sulfide (PPS) Information provided by PolyOne |
|||
Melt Temperature | 304 - 332 °C | 579 - 630 °F | |
PolyOne Edgetek® SF2-40CF/000 NATURAL Polyphenylene Sulfide (PPS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 304 - 332 °C | 579 - 630 °F | |
PolyOne Edgetek® SF-40CF/000 Polyphenylene Sulfide (PPS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 304 - 332 °C | 579 - 630 °F | |
PolyOne LubriOne™ PC-30CF/20T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 304 - 332 °C | 579 - 630 °F | |
LNP NORYL® EXCP0111 PPS + Polyphenylene Ether, 42% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Melt Temperature | 304 - 332 °C | 579 - 630 °F | |
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Melt Temperature | 135 - 332 °C | 275 - 630 °F | Average value: 298 °C Grade Count:91 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Melt Temperature | 304 - 332 °C | 580 - 630 °F | Molding |
PolyOne Lubri-Tech™ SF-10CF/15T Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
PolyOne Lubri-Tech™ SF-25GF/13T BLACK Polyphenylene Sulfide (PPS), Glass Filled, PTFE Lubricated
(discontinue Description/Features:Glass Fiber ReinforcedPTFE LubricatedBlackPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
PolyOne Lubri-Tech™ SF-25GF/13T-2S Polyphenylene Sulfide (PPS), Glass Filled, PTFE/Silicone Lubricated
(disco Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 332 °C | 600 - 630 °F | Molding |
PolyOne Lubri-Tech™ SF-30CF/13T2S Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE/Silicone Lubricated
&n Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
PolyOne Edgetek® SF-30GF-25MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
PolyOne Edgetek® SF-35GF-15MC/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
PolyOne Edgetek® SF-35GF-25MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedUL 94 V0 (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
PolyOne Edgetek® SF-40GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
PolyOne Edgetek® SF-40GF-10 MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 299 - 332 °C | 570 - 630 °F | |
PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled
(disco Information provided by PolyOne™ Corporation |
|||
Melt Temperature | 310 - 332 °C | 590 - 630 °F | |
LTL Color Compounds ColorFast® PC60 Polycarbonate 6 melt extrusion gradeAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 310 - 332 °C | 590 - 630 °F | |
LTL Color Compounds ColorFast® PCGF110 Polycarbonate, 10% Glass-Filled High modulus 10% glass-filled polycarbonate, V2-rated, general purposeAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 293 - 332 °C | 559 - 630 °F | |
Covestro Makrolon® DP 1-1456 Polycarbonate, Impact Grade Impact modified injection molding grade, extremely easy flow and easy mold release, for thin walled applications with long flow lengths.Information provided by Bayer.As of 1 September 2015, Bayer Ma.. |
|||
Melt Temperature | 315 - 332 °C | 599 - 630 °F | Extrusion Coating Processability |
Dow 4010 Low Density Polyethylene (LDPE) Polyethylene 4010 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry and moist foods packaging, sugar pouches, lidding stoc.. |
|||
Melt Temperature | 315 - 332 °C | 599 - 630 °F | Extrusion Coating Processability |
Dow 722 Low Density Polyethylene (LDPE) Polyethylene 722 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry foods packaging, snack foods packaging, moist foods pac.. |
|||
Melt Temperature | 310 - 332 °C | 590 - 630 °F | |
LTL Color Compounds ColorFast® FRPC310 Polycarbonate, Flame-Retarded V0-rated 10% glass-filled polycarbonate, excellent impact strengthAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 299 - 332 °C | 570 - 630 °F | Molding |
PolyOne Edgetek® SF-35GF-25MN/000 L Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |