Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.00020 - 0.00080 cm/cm

@Thickness 3.18 mm
0.00020 - 0.00080 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.00040 - 0.00080 cm/cm

@Thickness 3.18 mm
0.00040 - 0.00080 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 207 MPa
30000 psi
5.1 mm/min; ASTM D638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
5.1 mm/min; ASTM D638
Tensile Modulus 30.5 GPa
4420 ksi
5.1 mm/min; ASTM D638
Flexural Strength 283 MPa
41000 psi
ASTM D790
Flexural Modulus 25.8 GPa
3740 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 272 °C
522 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 10000 ohm-cm
100 - 10000 ohm-cm
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 304 - 332 °C
579 - 630 °F
Descriptive Properties Value Comments
Features Good Chemical Resistance
High Heat Resistance
High Rigidity
Linear Polymer Structure
Semi Crystalline
Filler / Reinforcement Carbon Fiber Reinforcement, 40% Filler by Weight
Forms Pellets
Generic Material PPS
Generic Name Polyphenylene Sulfide (PPS)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Aerospace Applications
Aircraft Applications
Automotive Applications
High Temperature Applications
Industrial Applications
Copyright © lookpolymers.com All Rights Reserved