Polymer Property : Gel Time = 30.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 30.0 - 60.0 min
30.0 - 60.0 min
Resin Technology Group FDA-24N Two component Polyurethane Adhesive
Resin Technology Group FDA-24N Two component Polyurethane AdhesiveFDA approvable, 1:1 ratio, general purpose adhesive
Gel Time 30.0 min
30.0 min
Slow
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer
EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria..
Gel Time 30.0 min
30.0 min
75°C
ACC EP RAP 60 EPI Engineered Polymers Aliphatic Polyurea
EP RAP 60 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, coating (silicone optional) developed for UV stable (colorfast) polyurea flooring applic..