Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Gel Time = 45.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 45.0 - 60.0 min

@Temperature 60.0 °C
45.0 - 60.0 min

@Temperature 140 °F
with 0.2%wt catalyst load
Hybrid Plastics FireQuench® PM 1287 Resin
FireQuench® PM1287 is an optically transparent, fire retardant hybrid nanocomposite resin that can serve as a replacement for standard epoxy-vinyl ester and related resins. It can be employed as ..
Gel Time 45.0 min
45.0 min
ACC QGel 310 QSI Quantum Silicones High Strength Gel
QGel 310 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid..
Gel Time 45.0 min
45.0 min
catalyzed with Deep Section Catalyst or 100: 0.5 for DBT Catalyst
ACC QSil 940 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting
QSil 940 is a special purpose, two-component condensation cure siloxane elastomer that exhibits excellent release properties unless a primer is used which results in excellent adhesion. The material..
Gel Time 45.0 min
45.0 min
catalyzed, DBT Catalyst
ACC QSil 40 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting
QSil 40 is a general purpose two-part, room temperature, condensation cure siloxane elastomer. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section Catalyst by weight. Cure speed..
Gel Time 45.0 min
45.0 min
ACC QSil 60 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting
QSil 60 is a red, high temperature, self-leveling, two-component, silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section ..