Material Notes:
PERMABOND UV670 is a single part, fast curing, UV curable adhesive. The cured adhesive is tough, flexible and has excellent impact resistance. Permabond UV670 is well suited for bonding glass to metals and metalized plastics Features & Benefits: Cure on demand Non-drip Flexible, good impact resistance Fast curing with low-power lamps 100% solids, no solvents Excellent adhesion to metal and glass Information provided by Permabond.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
uncured
Viscosity 2000 - 3000 cP

@Temperature 25.0 °C
2000 - 3000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
Tensile Strength 12.0 MPa
1740 psi
ASTM D2095
Elongation at Break 85 %
85 %
Adhesive Bond Strength 8.00 - 9.00 MPa
1160 - 1310 psi
Glass/steel, Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Optical Properties Metric English Comments
Refractive Index 1.47
1.47
Electrical Properties Metric English Comments
Dielectric Constant 4.0

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
4.0

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Dielectric Strength 12.0 kV/mm
305 kV/in
Processing Properties Metric English Comments
Cure Time 0.117 min
0.00194 hour
fixture time, (low power 4mW lamp)
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Cure Wavelength (nm) 365-400
Maximum Gap Fill (mm) 0.5
Strength Retention 10% at 200°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 150°C
Relative to 0°C
75% at 100°C
Relative to 0°C
95% at 50°C
Relative to 0°C