Processing Properties Metric English Comments
Cure Time 0.0333 - 0.0833 min
0.000556 - 0.00139 hour
With primer (Fixture)
ND Industries 226 Structural Adhesive
Light Cure Structural Adhesive gel
Cure Time 0.0333 - 0.0833 min
0.000556 - 0.00139 hour
With Excel 600392 primer under UV light (Fixture)
ND Industries 230 Structural Adhesive
Multi Cure, High Viscosity Adhesive
Cure Time 0.0333 - 0.0833 min
0.000556 - 0.00139 hour
Buna N Rubber, handling time
Permabond 101 Cyanoacrylate, Wicking Viscosity
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya..
Cure Time 0.0500 - 0.0833 min
0.000833 - 0.00139 hour
Steel, handling time
Permabond 101 Cyanoacrylate, Wicking Viscosity
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya..
Cure Time 0.0333 - 0.0833 min
0.000556 - 0.00139 hour
Neoprene, handling time
Permabond 940 Cyanoacrylate, low odor
PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.0500 - 0.0833 min
0.000833 - 0.00139 hour
Buna N Rubber, set time
Permabond 930 Cyanoacrylate
PERMABOND 930 is a low odor, non­fogging, non­frosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The ..
Cure Time 0.0500 - 0.0833 min
0.000833 - 0.00139 hour
Rubber set time
Lord Adhesives 6900 Medium Viscosity, Low Odor, Low Bloom Butyl Cyanoacrylate Adhesive
Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal..
Cure Time 0.0667 - 0.0833 min
0.00111 - 0.00139 hour
Plastic set time
Lord Adhesives 8400 Fast Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive
Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal..
Cure Time 0.0667 - 0.0833 min
0.00111 - 0.00139 hour
Plastic set time
Lord Adhesives 9900 Normal Setting, High Viscosity, Odorless, Non-Frosting Methyl Cyanoacrylate Adhesive
Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal..
Cure Time 0.0333 - 0.0833 min
0.000556 - 0.00139 hour
Neoprene, handling time
Permabond 941 Cyanoacrylate, low odor
PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..
Cure Time 0.0333 - 0.0833 min
0.000556 - 0.00139 hour
Neoprene, handling time
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..