Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | With primer (Fixture) |
ND Industries 226 Structural Adhesive Light Cure Structural Adhesive gel |
|||
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | With Excel 600392 primer under UV light (Fixture) |
ND Industries 230 Structural Adhesive Multi Cure, High Viscosity Adhesive |
|||
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | Buna N Rubber, handling time |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Steel, handling time |
Permabond 790 Cyanoacrylate, Surface insensitive PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Buna Rubber, set time |
Permabond 790 Cyanoacrylate, Surface insensitive PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Phenolic, set time |
Permabond 790 Cyanoacrylate, Surface insensitive PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | Neoprene, handling time |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Steel, handling time |
Permabond 791 Cyanoacrylate, Surface insensitive PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Buna N Rubber, handling time |
Permabond 791 Cyanoacrylate, Surface insensitive PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Phenolic, handling time |
Permabond 791 Cyanoacrylate, Surface insensitive PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Cure Time | 0.0333 - 0.0667 min | 0.000556 - 0.00111 hour | Plastic set time |
Lord Adhesives 5000 Fast Setting, High Elasticity, Low Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.0333 - 0.0667 min | 0.000556 - 0.00111 hour | Rubber set time |
Lord Adhesives 5000 Fast Setting, High Elasticity, Low Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Plastic set time |
Lord Adhesives 8300 Medium Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Rubber set time |
Lord Adhesives 8400 Fast Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.0333 min | 0.000556 hour | Hot tack |
Valley Adhesives EM-800 High Temperature Application Glue Stick Valley Adhesives EM-800 High Temperature Application Glue StickGood hot tack for packaging. |
|||
Cure Time | <= 0.0333 min | <= 0.000556 hour | |
Dymax 3-3073 Flexible Potting Ultra Fast™ Adhesives for Wire Harness, Strain Relief, Coil Coating and TerminatingCost EffectiveUltra Light-Weld® UV/Visible adhesives set in as little as one secondOn a material cost per applica.. |
|||
Cure Time | <= 0.0333 min | <= 0.000556 hour | |
Dymax 4-425 Glass Bonding Adhesive Ultra Fast™ Adhesives for Wire Harness, Strain Relief, Coil Coating and TerminatingCost EffectiveUltra Light-Weld® UV/Visible adhesives set in as little as one secondOn a material cost per applica.. |
|||
Cure Time | 0.0333 - 0.167 min | 0.000556 - 0.00278 hour | 10-20 mil thick layers cured with Dymax 5000-EC at 2 inches. Thicker layers may require more cure time. |
Dymax 9001v3.0 Low Modulus Clear Microencapsulant High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9001v3.0 Low Modulus Clear MicroencapsulantLowest stress potting and encapsulation on ceramic, FR-4 or flexible PCBs.. |
|||
Cure Time | 0.0333 - 0.250 min | 0.000556 - 0.00417 hour | 10-20 mil thick layers cured with Dymax 5000-EC at 2 inches. Thicker layers may require more cure time. |
Dymax 9001v3.1 Resilient, Low Modulus Clear Microencapsulant High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9001v3.1 Resilient, Low Modulus Clear MicroencapsulantLowest stress potting and encapsulation on ceramic, FR-4 or fl.. |
|||
Cure Time | 0.0333 - 0.167 min | 0.000556 - 0.00278 hour | 10-20 mil thick layers cured with Dymax 5000-EC at 2 inches. Thicker layers may require more cure time. |
Dymax 9001v3.5 Low Modulus Clear Microencapsulant High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9001v3.5 Low Modulus Clear MicroencapsulantLowest stress potting and encapsulation on ceramic, FR-4 or flexible PCBs.. |
|||
Cure Time | <= 0.0333 min | <= 0.000556 hour | |
Dymax 910 Strain Relief, Wire and Parts Tacking Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 910 Strain Relief, Wire and Parts Tacking AdhesiveFlexible, good adhesion and mechanical removable Cure Type: UV |
|||
Cure Time | <= 0.0333 min | <= 0.000556 hour | |
Dymax 914-A Strain Relief, Wire and Parts Tacking Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 914-A Strain Relief, Wire and Parts Tacking AdhesiveFaster curing, good insulation qualities, shock absorbing, deep .. |
|||
Cure Time | <= 0.0333 min | <= 0.000556 hour | |
Dymax 952 Potting and Encapsulation Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 952 Potting and Encapsulation AdhesiveFast curing, high strength, flexible, excellent moisture resistance. Cure Typ.. |
|||
Cure Time | 0.0333 - 0.333 min | 0.000555 - 0.00555 hour | Time to Handling Strength |
3M Scotch-Weld™ SI40 Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI40 (formerly SB95) is a low v.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Steel, handling time |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Buna N Rubber, handling time |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Cure Time | 0.0333 - 0.0500 min | 0.000556 - 0.000833 hour | Phenolic, handling time |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | Neoprene, handling time |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | Neoprene, handling time |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |