Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | With primer (Fixture) |
ND Industries 226 Structural Adhesive Light Cure Structural Adhesive gel |
|||
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | With Excel 600392 primer under UV light (Fixture) |
ND Industries 230 Structural Adhesive Multi Cure, High Viscosity Adhesive |
|||
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | Buna N Rubber, handling time |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Cure Time | 0.0500 - 0.0833 min | 0.000833 - 0.00139 hour | Steel, handling time |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | Neoprene, handling time |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Cure Time | 0.0500 - 0.0833 min | 0.000833 - 0.00139 hour | Buna N Rubber, set time |
Permabond 930 Cyanoacrylate PERMABOND 930 is a low odor, nonfogging, nonfrosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The .. |
|||
Cure Time | 0.0500 - 0.0833 min | 0.000833 - 0.00139 hour | Rubber set time |
Lord Adhesives 6900 Medium Viscosity, Low Odor, Low Bloom Butyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.0667 - 0.0833 min | 0.00111 - 0.00139 hour | Plastic set time |
Lord Adhesives 8400 Fast Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.0667 - 0.0833 min | 0.00111 - 0.00139 hour | Plastic set time |
Lord Adhesives 9900 Normal Setting, High Viscosity, Odorless, Non-Frosting Methyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | Neoprene, handling time |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Cure Time | 0.0333 - 0.0833 min | 0.000556 - 0.00139 hour | Neoprene, handling time |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |