Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lord Adhesives 8400 Fast Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Lord Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives 8400 Fast Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metals and plastics. Lord Cyanoacrylate Adhesives offer these benefits: Instant Cure. Lord Cyanoacrylate Adhesives develop strong bonds with setting times ranging from 5 to 130 seconds. Ease of Use. Lord Cyanoacrylate Adhesives are one-component systems that facilitate set-up and minimize production costs. Good Environmental Resistance. Lord Cyanoacrylate Adhesives offer excellent resistance to weathering and aging.Lord Adhesives 8400 Fast Setting, Medium Viscosity Ethyl Cyanoacrylate AdhesiveFast setting. Medium viscosity. For bonding most plastic and elastomeric materials. Excellent drop control and ability to bridge small tolerances. Well-suited for bonding most porous substrates such as foam rubber. MIL-A-46050C Type II, Class 2 Approved.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0382 lb/in³
Viscosity 210 cP
210 cP
Processing Properties Metric English Comments
Cure Time 0.0333 - 0.0500 min
0.000556 - 0.000833 hour
Rubber set time
0.0667 - 0.0833 min
0.00111 - 0.00139 hour
Plastic set time
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved